EN 1.0352 Structural and constructional steels
Data updates
This material has 595 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
EN 1.0352 Chemical Composition
EN 10222-2: 2017 / Steel forgings for pressure purposes - Part 2: Ferritic and martensitic steels with specified elevated temperature properties
Looking for full material performance data?
Free registration required • Instant access
EN 1.0352 Physical Properties
Temperature
This material has 595 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
EN 1.0352 Heat Treatments
- Annealed (+A): 890-930°C, cooled in furnace.
Normalized (+N): 890-930°C, cooled in air.
Normalized and tempered (+NT) or Quenched and tempered (+QT): 890 to 930°C, cooled in air, oil, polymer or water and tempered at 600-640°C, cooled in air or furnace.
EN 1.0352 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
249 Cross References
-
15 Composition
-
22 Mechanical Properties
-
3 Physical Properties
-
1 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
1 Creep
-
- Joints
-
- Coatings
-
143 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
161 Total Suppliers