G10MnMoV6-3 (European Union / EN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Cast steels
Country/Standard:
European Union / EN
Data updates
Latest Update: 2016-04
Total number of updates: 3
Update History:
2015-05
2015-01
Mechanical Properties
Temperature
Physical Properties
Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.
Register NowComposition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.12
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2
EN 10293: 2015 / Steel castings for general engineering uses
Heat Treatments
- (+QT1) Normalizing or austenitizing from 950 to 980ºC and colling in air; tempering from 640 to 660ºC; (+QT2) Normalizing or austenitizing from 950 to 980ºC and colling in liquid; tempering from 640 to 660ºC; (+QT3) Normalizing or austenitizing from 950 to 980ºC and colling in liquid; tempering from 740 to 760ºC and from 600 to 650ºC.
- Quenched and tempered: (+QT1) quenched from 950 to 980°C, cooled in air (for information only) and tempered from 640 to 660°C;<br />(+QT2) quenched from 950 to 980°C, cooled in liquid (for information only) and tempered from 640 to 660°C;<br />(+QT3) quenched from 950 to 980°C, cooled in liquid (for information only) and tempered from 600 to 650°C (referring to impact value at 20°C) or tempered from 740 to 760°C (referring to impact value on -20°C).
-
43 Cross References
-
20 Composition
-
78 Mechanical Properties
-
- Physical Properties
-
2 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
40 Total Suppliers