EN G24Mn6 Cast steels
Other designations:
Material group:
Ferrous Alloys / Cast steels
Country/Standard:
European Union / EN
Data updates
Latest Update: 2016-10
Total number of updates: 2
Update History
2015-05
EN G24Mn6 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.20 – 0.25
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Cu
VALUE
≤ 0.30
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Mn
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Ni
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
P
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
View Complete Material Data ›EN G24Mn6 Physical Properties
Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.
Register NowThis material has 147 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
EN G24Mn6 Heat Treatments
- (+QT1) Normalizing or austenitizing from 880 to 950ºC and colling in liquid; tempering from 520 to 570ºC; (+QT2) Normalizing or austenitizing from 880 to 950ºC and colling in liquid; tempering from 600 to 650ºC; (+QT3) Normalizing or austenitizing from 880 to 950ºC and colling in liquid; tempering from 650 to 680ºC.
- Quenched and tempered: (+QT1) quenched from 880 to 950°C, cooled in liquid (for information only) and tempered from 520 to 570°C;<br />(+QT2) quenched from 880 to 950°C, cooled in liquid (for information only) and tempered from 600 to 650°C;<br />(+QT3) quenched from 880 to 950°C, cooled in liquid (for information only) and tempered from 650 to 680°C.
EN G24Mn6 Mechanical Properties
Temperature
Impact Energy
val1
Full data available with free access
View Complete Material Data
J
Unlock full details
Mechanical properties are available with full access.
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›-
39 Cross References
-
31 Composition
-
34 Mechanical Properties
-
- Physical Properties
-
3 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
40 Total Suppliers