EN GS240 Cast steels
Data updates
This material has 9232 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
EN GS240 Chemical Composition
EN 10293: 2015 / Steel castings for general engineering uses
Looking for full material performance data?
Free registration required • Instant access
EN GS240 Heat Treatments
- Normalized (+N): 880 to 980°C; Cooled in air (for information only).
- Normalizing or austenitizing from 900 to 980ºC and colling in air.
EN GS240 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
EN GS240 International Equivalent Materials
Showing 15 of 332 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 332 international equivalents?
See all 332 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 332Cross References
- 22Composition
- 8Mechanical Properties
- -Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- 83Joints
- -Coatings
- -Dimensions
- 1Tribology
- 8491Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 293Total Suppliers