DIN 15 Mo 3 Structural and constructional steels
Data updates
This material has 689 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 15 Mo 3 Chemical Composition
DIN 17175: 1979 / Seamless Tubes of Heat-resistant Steels - Technical Conditions of Delivery
Looking for full material performance data?
Free registration required • Instant access
DIN 15 Mo 3 Physical Properties
Temperature
This material has 689 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 15 Mo 3 Heat Treatments
- Hot forming at 1100 - 850°C. The temperature can drop to 750°C during processing. Normalizing at 910 - 940°C.
- Hot working: 1100-850°C; Normalizing: 910-940°C
DIN 15 Mo 3 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 15 Mo 3 International Equivalent Materials
Showing 15 of 177 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 177 international equivalents?
See all 177 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 177Cross References
- 45Composition
- 138Mechanical Properties
- 52Physical Properties
- 7Heat Treatment
- -Metallography
- -Machinability
- 2Stress-Strain
- -Formability
- 24Fatigue
- -Fracture
- 5Creep
- 96Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 143Total Suppliers