DIN 54SiCr6 Structural and constructional steels
Data updates
This material has 348 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 54SiCr6 Chemical Composition
DIN 17221: 1988 / Hot rolled steels for springs suitable for quenching and tempering - Technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN 54SiCr6 Physical Properties
Temperature
This material has 348 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 54SiCr6 Heat Treatments
- Hardening temperature for end quenched test: 850 +/-5°C
- Hardening (cooling in oil): 830-860°C
DIN 54SiCr6 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN 54SiCr6 International Equivalent Materials
Showing 15 of 191 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 191 international equivalents?
See all 191 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 191Cross References
- 12Composition
- 11Mechanical Properties
- 3Physical Properties
- 5Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 6Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 120Total Suppliers