DIN X210Cr12 Tool steels
Data updates
This material has 253 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN X210Cr12 Chemical Composition
EN ISO 4957: 2018 / Tool steels
Looking for full material performance data?
Free registration required • Instant access
DIN X210Cr12 Physical Properties
Temperature
This material has 253 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN X210Cr12 Heat Treatments
- Austenitized at 970 +/- 10°C and oil quenched.
Tempered at 180 +/- 10°C. - Hardening (quencing in oil or hot bath): 940-970°C; Tempering: 180°C
DIN X210Cr12 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
DIN X210Cr12 International Equivalent Materials
Showing 15 of 86 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 86 international equivalents?
See all 86 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 86Cross References
- 12Composition
- 15Mechanical Properties
- 16Physical Properties
- 14Heat Treatment
- 3Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 6Dimensions
- 8Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 93Total Suppliers