DIN C50R Structural and constructional steels
Data updates
This material has 932 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN C50R Chemical Composition
EN 10083-1: 1991 / Quenched and tempered steels - Part 1: Technical delivery conditions for special steels (includes amendment A1:1996)
Looking for full material performance data?
Free registration required • Instant access
DIN C50R Physical Properties
Temperature
This material has 932 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN C50R Heat Treatments
- Hardening: 810-850°C (Temperatures at the lower end of the range are generally used for water, and those at the upper end for oil quenching; Time for austenitizing as a guide: at least 30 min.);
Quenching agent: Oil or water (Other quenching agents such as synthetic quenchants may also be used.);
Tempering: 550-660°C (Time for tempering as a guide: at least 1h.);
End quench test austenitizing: 850 ± 5°C (Time for austenitizing as a guide: 30-35 min.);
Normalizing: 830-870°C. - Austenitizing (quenching in water or oil): 810-850°C, t > 30 min. NOTE: The temperatures at the lower end of the range are generally applicable to hardening in water and those at the upper end for hardening in oil. Synthetic quenchants may also be used. Tempering: 550-660°C, t > 60 min. A mandatory end quench test shall be carried out at 850+/- 5°C. Normalizing: 830-870°C, t > 30 min.
DIN C50R Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
399 Cross References
-
57 Composition
-
201 Mechanical Properties
-
3 Physical Properties
-
6 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
10 Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
6 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
250 Total Suppliers