C 10 (Germany / DIN) Material Properties

Other designations:
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2015-04
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 310 — 760 MPa view details
Elongation, A 7 % view details
Brinell Hardness (HB) 92 — 163 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 45 — 110.2 ksi view details
Elongation, A 7 % view details
Brinell Hardness (HB) 92 — 163 view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.0600 – 0.1200
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.2500 – 0.5000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.0450
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

DIN 1652-3: 1990 / Bright steel made from case hardening steel; technical delivery conditions

Heat Treatments

  • Carburizing at 880 - 980°C. Core-hardening at 880 - 920°C, case hardening at 780 - 820°C, quenching. Tempering at 150 - 200°C.
  • Hot working 1150-850°C; Soft annealing 650-700°C; Carburize 900-950°C; Temper 150-180°C/min. (1 h)