DIN 1.5805 Structural and constructional steels
Data updates
This material has 157 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DIN 1.5805 Chemical Composition
EN 10084: 2008 / Case hardening steels - Technical delivery conditions
Looking for full material performance data?
Free registration required • Instant access
DIN 1.5805 Physical Properties
Temperature
This material has 157 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DIN 1.5805 Heat Treatments
- End quench test: Quench from 880°C. Carburizing: 875 to 925°C; NOTE: If steels are direct hardened, in general, a carburizing temperature of 950°C is not exceeded. For special procedures, for example under vacuum, higher temperatures (for example 1020 to 1050°C) are not unusual. Core hardening: 830 to 860°C; Case hardening: 780 to 810°C; Tempering: 150 to 200°C (as a guide, for 1 hour minimum).
DIN 1.5805 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book a Demo
-
55 Cross References
-
16 Composition
-
21 Mechanical Properties
-
3 Physical Properties
-
4 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
5 Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
- Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
53 Total Suppliers