DIN 1.5508 Structural and constructional steels

Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2020-05
Total number of updates: 3
Update History
2018-01 2015-07

This material has 249 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.5508 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
B
VALUE
0.0008 – 0.0050
UNIT
%
CAS NUMBER
7440-42-8
CRITERIA
C
VALUE
0.1900 – 0.2500
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.5000 – 0.8000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

DIN 1654-4: 1989 / Cold heading and cold extruding steels; technical delivery conditions for steels for quenching and tempering

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.5508 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.67 — 7.86 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 249 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

DIN 1.5508 Heat Treatments

  • Austenizing temperature: 890 ± 5°C
  • Hardening (quenching in water or oil): 860-890°C; Tempering: 550-660°C; Normalizing: 880-910°C

DIN 1.5508 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≤ 690 MPa
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
55 %
Unlock full details
Full data available with free access View Complete Material Data
Rockwell Hardness (HR)
≤ 40
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book a Demo

  • 103 Cross References

  • 14 Composition
  • 25 Mechanical Properties
  • 3 Physical Properties
  • 8 Heat Treatment
  • - Metallography
  • - Machinability

  • - Stress-Strain
  • - Formability
  • - Fatigue
  • - Fracture
  • - Creep

  • - Joints
  • - Coatings
  • - Dimensions
  • - Tribology

  • - Corrosion
  • - Ageing
  • - Weatherability
  • - Irradiation

  • 96 Total Suppliers