1.3207 (Germany / DIN) Material Properties
Other designations:
, ,
Material group:
Ferrous Alloys / Tool steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2023-10
Total number of updates: 4
Update History:
2023-01
2022-12
2019-05
Mechanical Properties
Temperature
Physical Properties
Temperature
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE)
val1
Full data access requires a free trial.
Sign Up Free
10-6/°F
view details
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.20 – 1.35
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Co
VALUE
9.5 – 10.5
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Cr
VALUE
3.8 – 4.5
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
V
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-62-2
CRITERIA
W
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-33-7
EN ISO 4957: 2018 / Tool steels
Heat Treatments
- <b>Soft annealing</b>: Heated slowly at 770-840°C (the upper limit of this temperature range applies to higher alloyed, and the lower limit for lower alloyed high speed steels), held for 2 to 4 hours, slowly cooled in the furnace to 500-600°C, removed from the furnace and placed in a protected place. <br /><br /><b>Hardening</b>: Heated at 1210-1250°C. The temperature of the hot bath should be 500-550°C and must not exceed 580°C during extended use. <br /> When cooling in oil, at about 40-70°C, the samples should be moved slowly and evenly and should not be left in oil until completely cooled, but when they reach 300-200°C. <br /><br /> <b>Tempering</b>: Heated slowly at 540-570°C, held for 1 to 3 hours, depending on the size of the samples. The tempering takes place in a neutral salt bath or in an air circulation furnace.
- Austenitized at 1230 ± 10°C and quenched. Usual quenching media in practice are air, gas or salt bath. Total heating time of test pieces in a salt bath is 3 min. for hardening and minimum 2 periods of 60 min. each for tempering.<br />Tempered at 560 ± 10°C.
-
71 Cross References
-
26 Composition
-
18 Mechanical Properties
-
18 Physical Properties
-
16 Heat Treatment
-
- Metallography
-
- Machinability
-
- Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
14 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-
63 Total Suppliers