1.1152 (Germany / DIN) Material Properties

Other designations: ,
Material group: Ferrous Alloys / Structural and constructional steels
Country/Standard: Germany / DIN

Data updates

Latest Update: 2025-02
Total number of updates: 3
Update History:
2020-03 2018-01

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 300 MPa view details
Tensile Strength 450 MPa view details
Elongation, A 20 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
J
view details
Yield Strength, Rp0.2 43.5 ksi view details
Tensile Strength 65.3 ksi view details
Elongation, A 20 % view details
Reduction of Area val1
Full data access requires a free trial. Sign Up Free
%
view details
Impact Energy val1
Full data access requires a free trial. Sign Up Free
ft·lb
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 190 — 210 GPa view details
Density 7.67 — 7.86 kg/dm³ view details
Poisson Coefficient 0.27 — 0.3 view details
Modulus of Elasticity 27.6 E+03 — 30.5 E+03 ksi view details
Density 0.277 — 0.284 lb/in³ view details
Poisson Coefficient 0.27 — 0.3 view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.1700 – 0.2400
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.3000 – 0.6000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
P
VALUE
≤ 0.0350
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
S
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

DIN 1654-4: 1989 / Cold heading and cold extruding steels; technical delivery conditions for steels for quenching and tempering

Heat Treatments

  • Hardening (quenching in water) : 860-890°C; Tempering: 540-680°C; Normalizing: 880-910°C