1.0722 (Germany / DIN) Material Properties
Other designations:
Material group:
Ferrous Alloys / Structural and constructional steels
Country/Standard:
Germany / DIN
Data updates
Latest Update: 2024-12
Total number of updates: 2
Update History:
2018-08
Mechanical Properties
Temperature
Physical Properties
Temperature
Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.07 – 0.13
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Mn
VALUE
0.70 – 1.10
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Other
VALUE
Elements such as Te, Bi etc., may only be added by the manufacturer for improving machinability
UNIT
%
CAS NUMBER
CRITERIA
P
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7723-14-0
CRITERIA
Pb
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
S
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7704-34-9
CRITERIA
Si
VALUE
val1
Full data access requires a free trial.
Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
EN 10087: 1998 / Free-cutting steels - Technical delivery conditions for semi-finished products, hot-rolled bars and rods
Heat Treatments
- Carburizing: 880-980°C. The carburizing temperature will depend on the chemical composition of the steel, the mass of the product, and the carburizing medium. If the steels are direct hardened, in general, a temperature of 950°C is not exceeded. For special procedures, for example under vacuum, higher temperatures (for example 1 020 to 1 050°C) are not unusual; <br /> Core-hardening: 880-920°C. When applying the single quench method, the steel is to be quenched from the carburizing temperature or a lower temperature. The lower hardening temperatures are in each case to be preferred, in particular when there is risk of distortion; Case-hardening: 780-820°C;<br /> Quenching agent: water, oil, emulsion. The kind of quenching agent depends on, for example, the shape of the products, the cooling conditions and the amount of furnace filling;<br /> Tempering: 150-200°C (1 h minimum).
- Operation of hardening - 880-920°C;Carburize 880-980°C; Operation of hardening - Heat up 780-820°C; Temper 150-200°C/min. 1 h
-
110 Cross References
-
31 Composition
-
97 Mechanical Properties
-
8 Physical Properties
-
2 Heat Treatment
-
- Metallography
-
- Machinability
-
20 Stress-Strain
-
- Formability
-
- Fatigue
-
- Fracture
-
- Creep
-
- Joints
-
- Coatings
-
2 Dimensions
-
- Tribology
-
- Corrosion
-
- Ageing
-
- Weatherability
-
- Irradiation
-