GB W6Mo5Cr4V3 Tool steels
Data updates
This material has 254 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
GB W6Mo5Cr4V3 Chemical Composition
GB/T 9943: 2025 / High-speed tool steels
Looking for full material performance data?
Free registration required • Instant access
GB W6Mo5Cr4V3 Physical Properties
Temperature
This material has 254 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
GB W6Mo5Cr4V3 Heat Treatments
- Preheat temperature: 800-900°C; Quenching temperature: 1190-1210°C (salt bath), 1200-1220°C (box furnace); Quenching medium: oil or salt bath; Tempering temperature: 550°C.
Tempering shall be performed three times: each time for 1 hour in a salt bath, and for 2 hours each in a box furnace or vacuum furnace.
GB W6Mo5Cr4V3 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
GB W6Mo5Cr4V3 International Equivalent Materials
Showing 15 of 124 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 124 international equivalents?
See all 124 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 124Cross References
- 20Composition
- 3Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 102Total Suppliers