CSN 17 021 Stainless steels
Data updates
This material has 527 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
CSN 17 021 Chemical Composition
CSN 41 7021: 1980 / Chromium steel 17 021
Looking for full material performance data?
Free registration required • Instant access
CSN 17 021 Physical Properties
Temperature
This material has 527 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
CSN 17 021 Heat Treatments
- Forging at 1150 to 850°C, gradually cooling;
Hardening at 930 to 1000°C, cooling in oil or air;
Tempering at 640 to 750°C, cooling in air;
Annealing at 760 to 800°C, cooling in furnace or air;
Normalizing at 960 to 1000, cooling in air;
Tempering after normalization annealing at 700 to 780°C, cooling in air;
CSN 17 021 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
CSN 17 021 International Equivalent Materials
Showing 15 of 261 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 261 international equivalents?
See all 261 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 261Cross References
- 8Composition
- 57Mechanical Properties
- 21Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 8Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 171Total Suppliers