Kingfa PA66-C200 NC110 (PROPRIETARY) Material Properties

Material group: Polymers / Plastics, thermoplasts / Polyamides (PA6, PA6T...) / PA66
Country/Standard: PROPRIETARY

Data updates

Latest Update: -
Total number of updates: 0
Update History:
-

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 48 — 68 MPa view details
Tensile Strain 22 — 50 % view details
Tensile Strain at Break 22 — 50 % view details
Flexural Strength 50 — 90 MPa view details
Impact Strength val1
Full data access requires a free trial. Sign Up Free
kJ/m²
view details
Charpy Notched Impact Strength val1
Full data access requires a free trial. Sign Up Free
kJ/m²
view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details
Tensile Strength 6.962 — 9.863 ksi view details
Tensile Strain 22 — 50 % view details
Tensile Strain at Break 22 — 50 % view details
Flexural Strength 7.25 — 13.05 ksi view details
Impact Strength val1
Full data access requires a free trial. Sign Up Free
ft·lb/in²
view details
Charpy Notched Impact Strength val1
Full data access requires a free trial. Sign Up Free
ft·lb/in²
view details
Rockwell Hardness (HR) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Flexural Modulus 1.1 — 2.3 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Volume Resistivity val1
Full data access requires a free trial. Sign Up Free
Ω·m
view details
Heat Deflection Temperature (HDT) 65 — 200 °C view details
Flammability Rating val1
Full data access requires a free trial. Sign Up Free
view details
Molding Shrinkage val1
Full data access requires a free trial. Sign Up Free
%
view details
Moisture Absorption 2.4 % view details
Modulus of Elasticity val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Flexural Modulus 160 — 334 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Volume Resistivity val1
Full data access requires a free trial. Sign Up Free
Ω∙circular·mil/ft
view details
Heat Deflection Temperature (HDT) 149 — 392 °F view details
Flammability Rating val1
Full data access requires a free trial. Sign Up Free
view details
Molding Shrinkage val1
Full data access requires a free trial. Sign Up Free
%
view details
Moisture Absorption 2.4 % view details

Composition

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now