DTD 5363 Titanium Alloys
Data updates
This material has 23 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DTD 5363 Chemical Composition
D.T.D. 5363: 1978 / Castings of titanium-aluminium-vanadium alloy (Annealed)
Looking for full material performance data?
Free registration required • Instant access
DTD 5363 Physical Properties
Temperature
This material has 23 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DTD 5363 Heat Treatments
- Anneal at a temperature between 700°C and 850°C in a protective (argon or vacuum) atmosphere for not less than 2 hours and furnace cool in a protective atmosphere to a temperature below 500°C, followed by air cooling to room temperature.
DTD 5363 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 12Composition
- 8Mechanical Properties
- 2Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers