DTD 5015A Magnesium Alloys
Data updates
This material has 19 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DTD 5015A Chemical Composition
D.T.D. 5015A: 1971 / Ingots and Castings of Magnesium - Zinc - Thorium - Zirconium Alloy (precipitation treated) (Zn 5.5, Th 1.8, Zr 0.7)
Looking for full material performance data?
Free registration required • Instant access
DTD 5015A Physical Properties
Temperature
This material has 19 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DTD 5015A Heat Treatments
- Heat at a temperature not exceeding 350°C for not less than 2 hours. Cool in air or quench in oil or water
DTD 5015A Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 10Composition
- 6Mechanical Properties
- 2Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers