Generic Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd Titanium Alloys
Material group:
Nonferrous Alloys / Titanium Alloys
Country / Standard:
Generic
Data updates
Latest Update: 2019-10
Total number of updates: 1
Update History
This material has 12 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
Generic Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
4.9 – 5.5
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
Mo
VALUE
1.0 – 1.5
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
Nb
VALUE
0.4
UNIT
%
CAS NUMBER
7440-03-1
CRITERIA
Nd
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-00-8
CRITERIA
Si
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Sn
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-31-5
CRITERIA
Ta
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-25-7
CRITERIA
Ti
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-32-6
CRITERIA
Zr
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-67-7
High-temperature tensile deformation behavior and microstructure evolution of Ti55 titanium alloy, Z. Liu, P. Li, L. Xiong, T. Liu, L. He, 2017
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
Generic Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd Physical Properties
Temperature
Modulus of Elasticity
80 — 130
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Density
4.3 — 5.1
kg/dm³
Unlock full details
Full data available with free access
View Complete Material Data
This material has 12 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
Generic Ti-5Al-4Sn-2Zr-1Mo-0.25Si-1Nd Heat Treatments
- After the final rolling at 960°C, the sheet was then annealed at 750°C for 60 min, and finally cooled to room temperature in a furnace.
Optimize material selection for your application - Book A Demo
- -Cross References
- 9Composition
- -Mechanical Properties
- 2Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers