PROPRIETARY VACODUR S Plus Cobalt Alloys
Material group:
Nonferrous Alloys / Cobalt Alloys
Country / Standard:
PROPRIETARY
Data updates
Latest Update: 2018-10
Total number of updates: 1
Update History
This material has 25 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY VACODUR S Plus Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Co
VALUE
49
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Fe
VALUE
49
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
V+Ta
VALUE
2
UNIT
%
CAS NUMBER
CRITERIA
Zr
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-67-7
Vacuumschmelze GmbH & Co. KG, Product Data Sheets,
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY VACODUR S Plus Physical Properties
Temperature
Modulus of Elasticity
250
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Resistivity
0.42
Ω∙mm²/m
Unlock full details
Full data available with free access
View Complete Material Data
Density
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Conductivity
Unlock full details
Full data available with free access
View Complete Material Data
Thermal Conductivity
32
W/(m∙°C)
Unlock full details
Full data available with free access
View Complete Material Data
This material has 25 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY VACODUR S Plus Heat Treatments
- Recommended parameters for the final heat treatment
Annealed I: Temperature 840°C; Holding time (strip) 4 h; Cooling rate 100-300 K/h.
Annealed II: Temperature 720°C; Holding time(strip) 1-2 h; Cooling rate 100-300 K/h.
PROPRIETARY VACODUR S Plus Mechanical Properties
Temperature
Tensile Strength
800 — 1200
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
6 — 8
%
Unlock full details
Full data available with free access
View Complete Material Data
Vickers Hardness (HV)
val1
Full data available with free access
View Complete Material Data
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
400 — 800
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- -Cross References
- 4Composition
- 8Mechanical Properties
- 9Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 2Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 1Total Suppliers