DTD 5005A Magnesium Alloys
Data updates
This material has 20 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
DTD 5005A Chemical Composition
D.T.D. 5005A: 1971 / Ingots and Castings of Magnesium - Thorium - Zinc - Zirconium Alloy (Precipitation treated) ( Th 3.0, Zn 2.2, Zr 0.7)
Looking for full material performance data?
Free registration required • Instant access
DTD 5005A Physical Properties
Temperature
This material has 20 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
DTD 5005A Heat Treatments
- The castings and test samples shall be heat treated together as follows:
- Heat at a temperature not exceeding 350°C for not less than 10 hours
- Cool in air or quench in oil or water
DTD 5005A Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1Cross References
- 10Composition
- 6Mechanical Properties
- 2Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers