Permenorm 5000 H2 (PROPRIETARY) Material Properties

Material group: Nonferrous Alloys / Nickel / Nickel Alloy
Country/Standard: PROPRIETARY

Data updates

Latest Update: 2021-07
Total number of updates: 2
Update History:
2017-02

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 850 — 1100 MPa view details
Vickers Hardness (HV) 220 — 300 view details
Tensile Strength 123.3 — 159.5 ksi view details
Vickers Hardness (HV) 220 — 300 view details

Physical Properties


Temperature

0 - 30°C
100 - 300°C
PROPERTY / VALUE
Modulus of Elasticity 185 — 205 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Thermal Conductivity 13 — 14 W/(m∙°C) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Electrical Resistivity 0.45 Ω∙mm²/m view details
Modulus of Elasticity 26.8 E+03 — 29.7 E+03 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Thermal Conductivity 7.51 — 8.09 BTU/(h∙ft∙°F) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Electrical Resistivity 748 E-06 Ω∙circular·mil/ft view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Co
VALUE
≤ 0.1
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Fe
VALUE
Balance
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Ni
VALUE
36 – 48
UNIT
%
CAS NUMBER
7440-02-0

Vacuumschmelze GmbH & Co. KG, Product Data Sheets / Available at: www.vacuumschmelze.com, visited 2017

Heat Treatments