CSN CuCd0.2 Copper Alloys

Material group: Nonferrous Alloys / Copper Alloys
Country / Standard: Czech Republic / CSN

Data updates

Latest Update: 2016-08
Total number of updates: 1
Update History

This material has 23 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CSN CuCd0.2 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Cd
VALUE
0.1000 – 0.3000
UNIT
%
CAS NUMBER
7440-43-9
CRITERIA
Cu
VALUE
Balance
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Other
VALUE
≤ 0.3000
UNIT
%
CAS NUMBER

CSN 42 3019: 1990 / Wrought соррег alloy CuCd0,2

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CSN CuCd0.2 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
100 — 150 GPa
Unlock full details
Full data available with free access View Complete Material Data
Electrical Resistivity
≤ 0.0203 Ω∙mm²/m
Unlock full details
Full data available with free access View Complete Material Data
Density
val1
Full data available with free access View Complete Material Data
kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Melting Temperature
val1
Full data available with free access View Complete Material Data
°C
Unlock full details
Full data available with free access View Complete Material Data
Electrical Conductivity
val1
Full data available with free access View Complete Material Data
S/m
Unlock full details
Full data available with free access View Complete Material Data

This material has 23 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

CSN CuCd0.2 Heat Treatments


  • Pressing at 920 to 940°C.
    Rolling at 860°C.

CSN CuCd0.2 Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≥ 450 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
≥ 2 %
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 3Composition
  • 12Mechanical Properties
  • 7Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • -Total Suppliers