PROPRIETARY Carpenter P6 Alloy Cobalt Alloys

Material group: Nonferrous Alloys / Cobalt Alloys
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2016-02
Total number of updates: 1
Update History

This material has 11 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Carpenter P6 Alloy Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Co
VALUE
45.00
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Fe
VALUE
Balance
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Ni
VALUE
6.00
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
V
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-62-2

Carpenter Technology Corporation, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Carpenter P6 Alloy Physical Properties


Temperature

PROPERTY / VALUE
Electrical Resistivity
0.33 Ω∙mm²/m
Unlock full details
Full data available with free access View Complete Material Data
Density
8.16 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Electrical Conductivity
3.03e+006 S/m
Unlock full details
Full data available with free access View Complete Material Data
Coefficient of Thermal Expansion (CTE)
val1
Full data available with free access View Complete Material Data
10-6/°C
Unlock full details
Full data available with free access View Complete Material Data

This material has 11 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY Carpenter P6 Alloy Heat Treatments


  • After fabricating to the desired form, the material should be degreased prior to final age hardening heat treatment. The material should then be placed into a furnace with a protective atmosphere and held at 550 to 600°C for two to five hours. This final heat treatment is necessary to obtain the desired magnetic characteristics of the material. Adjustment of the magnetic properties is possible via control of the final heat treatment.

PROPRIETARY Carpenter P6 Alloy Mechanical Properties


Temperature

PROPERTY / VALUE
Rockwell Hardness (HR)
55
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 4Composition
  • 1Mechanical Properties
  • 4Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers