WL 2.4672 Nickel Alloys
Data updates
This material has 35 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
WL 2.4672 Chemical Composition
WL 2.4672: 1981 / High temperature nickel cast alloy with about 0.06 C-20 Co-20 Cr-6 Mo-2 Ti-0.5 Al; investment casting
Looking for full material performance data?
Free registration required • Instant access
WL 2.4672 Physical Properties
Temperature
This material has 35 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
WL 2.4672 Heat Treatments
- Soft (with or without straightening or stretching) (.1)
Precipitation treated (solution heat- treated and artificially aged) (.7)
Solution heat treated: 1150±15°C, 2h, air.
Solution and precipitation treated: 800±10°C, 8h, air.
WL 2.4672 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
WL 2.4672 International Equivalent Materials
Showing 1 of 2 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 2 international equivalents?
See all 2 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 2Cross References
- 17Composition
- 7Mechanical Properties
- 8Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers