2.4478 (Germany / DIN) Material Properties

Other designations: ,
Material group: Nonferrous Alloys / Nickel / Nickel Alloy
Country/Standard: Germany / DIN

Data updates

Latest Update: 2024-10
Total number of updates: 7
Update History:
2024-03 2021-03 2020-12 2020-11 2020-02 2017-01

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 540 — 820 MPa view details
Elongation, A 30 % view details
Tensile Strength 78.3 — 118.9 ksi view details
Elongation, A 30 % view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
≥ 300°C
PROPERTY / VALUE
Modulus of Elasticity 160 — 205 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 17 W/(m∙°C) view details
Electrical Resistivity 0.43 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Modulus of Elasticity 23.2 E+03 — 29.7 E+03 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 9.82 BTU/(h∙ft∙°F) view details
Electrical Resistivity 715 E-06 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.0200
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Fe
VALUE
47.0000 – 50.0000
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mn
VALUE
≤ 0.6000
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3

DIN 17745: 2002 / Wrought alloys of nickel and iron - Chemical composition

Heat Treatments

  • Annealed at 800-1000°C, air or furnace cooled. Structure after heat treatment is austenitic.