PROPRIETARY Wieland-N32 Copper Alloys
Material group:
Nonferrous Alloys / Copper Alloys
Country / Standard:
PROPRIETARY
Data updates
Latest Update: 2020-10
Total number of updates: 2
Update History
2014-03
This material has 125 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Wieland-N32 Chemical Composition
CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Cu
VALUE
57
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Ni
VALUE
12
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Pb
VALUE
1
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
Zn
VALUE
val1
Full data available with free access
View Complete Material Data
UNIT
%
CAS NUMBER
7440-66-6
Wieland SMH GmbH, Product Data Sheets,
Looking for full material performance data?
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Wieland-N32 Physical Properties
Temperature
Modulus of Elasticity
100 — 150
GPa
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Resistivity
0.246
Ω∙mm²/m
Unlock full details
Full data available with free access
View Complete Material Data
Density
Unlock full details
Full data available with free access
View Complete Material Data
Electrical Conductivity
Unlock full details
Full data available with free access
View Complete Material Data
Melting Temperature
Unlock full details
Full data available with free access
View Complete Material Data
Thermal Conductivity
42
W/(m∙°C)
Unlock full details
Full data available with free access
View Complete Material Data
This material has 125 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
View Complete Material Data ›
Free registration required • Instant access
Free registration required • Instant access
PROPRIETARY Wieland-N32 Heat Treatments
- Hot working: 850 - 925°C; Soft annealing: 600 - 700°C, 1 - 3 h; Thermal stress relieving: 300 - 400°C, 1 - 3 h.
PROPRIETARY Wieland-N32 Mechanical Properties
Temperature
Tensile Strength
≥ 420
MPa
Unlock full details
Full data available with free access
View Complete Material Data
Brinell Hardness (HB)
110 — 190
Unlock full details
Full data available with free access
View Complete Material Data
Elongation, A
≥ 6
%
Unlock full details
Full data available with free access
View Complete Material Data
Yield Strength, Rp0.2
Unlock full details
Full data available with free access
View Complete Material Data
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
View Complete Material Data ›
Book A Demo
Free registration required • Instant access
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 43Cross References
- 4Composition
- 22Mechanical Properties
- 9Physical Properties
- 1Heat Treatment
- -Metallography
- 1Machinability
- 4Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 41Total Suppliers