UNI P-AG3.5 Aluminium Alloys
Data updates
This material has 105 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
UNI P-AG3.5 Chemical Composition
UNI 3575: 1955 / Primary wrought aluminium-magnesium alloy (Mg 3.5%)
Looking for full material performance data?
Free registration required • Instant access
UNI P-AG3.5 Physical Properties
Temperature
This material has 105 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
UNI P-AG3.5 Heat Treatments
- R: Full annealing for 2 to 4 hours at the temperature range of 360 - 400 °C. From a very hardened material (H 35) it is possible to obtain a less hardened material (H 15 - H 25) through partial annealing at 200 - 230 °C for 4 to 6 hours. Hot working range : 360 - 420 °C
UNI P-AG3.5 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
UNI P-AG3.5 International Equivalent Materials
Showing 12 of 13 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 13 international equivalents?
See all 13 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 13Cross References
- 10Composition
- 46Mechanical Properties
- 12Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- 15Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 8Total Suppliers