AIR 7075 Aluminium Alloys
Data updates
This material has 986 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AIR 7075 Chemical Composition
AIR 9048: 1978 / Test conditions for rolled aluminum alloy used in aerospace structures.
Looking for full material performance data?
Free registration required • Instant access
AIR 7075 Physical Properties
Temperature
This material has 986 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AIR 7075 Heat Treatments
- Delivery condition: F
State of a raw product, obtained by plastic deformation, hot or cold, without its mechanical characteristics being defined.
Delivery condition: T6
Solution heat-treated at 465°C ± 5°C, water quenched, max. temperature 40°C. Tempered at 135 ± 3°C, 12-16h.
Delivery condition: T73
Solution heat-treated at 465°C ± 5°C, water quenched, max. temperature 40°C. Tempered at 108 ± 5°C, 6-8h + 177°C ± 5°C, 8-12h.
Delivery condition: T7351
Solution heat-treated at 465°C ± 5°C, water quenched, max. temperature 40°C. Controlled traction: 1 to 3%. Tempered at 108 ± 5°C, 6-8h + 177°C ± 5°C, 8-12h.
Delivery condition: T76
Solution heat-treated at 465°C ± 5°C, water quenched, max. temperature 40°C. Tempered at 120 ± 5°C, 3-5h + 161°C ± 3 °C, 15-18h.
Delivery condition: T7651
Solution heat-treated at 465°C ± 5°C, water quenched, max. temperature 40°C. Controlled traction: 1 to 3%. Tempered at 120 ± 5°C, 3-5h + 161°C ± 3°C, 15-18h.
Used condition: T62
F + Solution heat-treated at 465°C ± 5°C and water quenched, max. temperature 40°C. Tempered at 135°C ± 3°C, 12-16h. - Solution heat treated and artificially aged (T6) - Solution heat treated, 465°C ± 5°, cooling in water, max. temperature 40°C and artificially aged 12 to 16h at 135°C ± 3°C.
Solution and precipitation heat treated (T76) - Solution heat treated, 465°C ± 5°, cooling in water, max. temperature 40°C and artificially aged 3 to 5h at 120°C ± 5°C + 15 to 18h at 161°C ± 3°C.
AIR 7075 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AIR 7075 International Equivalent Materials
Showing 15 of 198 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 198 international equivalents?
See all 198 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 198Cross References
- 24Composition
- 189Mechanical Properties
- 19Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- 131Stress-Strain
- 20Formability
- 262Fatigue
- 64Fracture
- 7Creep
- -Joints
- -Coatings
- 1Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 69Total Suppliers