PROPRIETARY IMI 318 Titanium Alloys
Data updates
This material has 4321 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY IMI 318 Chemical Composition
Smithells Metals Reference Book, Eds. E.A.Brandes, G.B.Brook, Butterworth Heinemann Publications, Oxford, 1999
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY IMI 318 Physical Properties
Temperature
This material has 4321 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY IMI 318 Heat Treatments
- Sheets: Annealed at 700°C/ 20 min/ AC; Descaled.
Plates; < 10 mm: Annealed at 700°C/ 20 min/ AC; Descaled and pickled.
Bars; 150 mm: Annealed at 700°C/ 2 hr/ 5 mm section/ AC.
PROPRIETARY IMI 318 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 2Cross References
- 3Composition
- 18Mechanical Properties
- 8Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- 1Fatigue
- -Fracture
- 1Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- 4283Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 4Total Suppliers