KS CAC706 Copper Alloys
Data updates
This material has 468 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
KS CAC706 Chemical Composition
D 6024: 2009 / Copper and copper alloy castings
Looking for full material performance data?
Free registration required • Instant access
KS CAC706 Physical Properties
Temperature
This material has 468 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
KS CAC706 Heat Treatments
- Solution treatment at 860-890℃ for 1h/in, water cooling, annealing at 620-660℃ for 2 hours, air cooling.
KS CAC706 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
KS CAC706 International Equivalent Materials
Showing 15 of 25 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 25 international equivalents?
See all 25 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 25Cross References
- 3Composition
- 8Mechanical Properties
- 2Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- 424Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 5Total Suppliers