Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 240 MPa view details
Elongation, A 1 % view details
Brinell Hardness (HB) 60 view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 34.8 ksi view details
Elongation, A 1 % view details
Brinell Hardness (HB) 60 view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
PROPERTY / VALUE
Modulus of Elasticity 69 — 79 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 130 — 160 W/(m∙°C) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.045 — 0.063 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Modulus of Elasticity 10 E+03 — 11.5 E+03 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Poisson Coefficient val1
Full data access requires a free trial. Sign Up Free
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 75.1 — 92.4 BTU/(h∙ft∙°F) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 75.6 E-06 — 104 E-06 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
Remainder
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
Cu
VALUE
≤ 0.10
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
≤ 1.0
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Other each
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Other total
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Ti
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-32-6
CRITERIA
Zn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-66-6

EN 1706: 2020 / Aluminium and aluminium alloys - Castings - Chemical composition and mechanical properties

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now