C 3604 (Korea / KS) Material Properties

Material group: Nonferrous Alloys / Copper
Country/Standard: Korea / KS

Data updates

Latest Update: 2015-06
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 335 MPa view details
Vickers Hardness (HV) 80 view details
Tensile Strength 48.6 ksi view details
Vickers Hardness (HV) 80 view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 100 — 150 GPa view details
Density 7.5 — 9.3 kg/dm³ view details
Modulus of Elasticity 14.5 E+03 — 21.8 E+03 ksi view details
Density 0.271 — 0.336 lb/in³ view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Cu
VALUE
57.0 – 61.0
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
≤ 0.50
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Fe+Sn
VALUE
≤ 1.0
UNIT
%
CAS NUMBER
CRITERIA
Pb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
Zn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-66-6