ASTM B 462 N08020 Nickel Alloys
Data updates
This material has 8420 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM B 462 N08020 Chemical Composition
B462: 2025 / Standard Specification for Forged or Rolled Nickel Alloy Pipe Flanges, Forged Fittings, and Valves and Parts for Corrosive High-Temperature Service
Looking for full material performance data?
Free registration required • Instant access
ASTM B 462 N08020 Physical Properties
Temperature
This material has 8420 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM B 462 N08020 Heat Treatments
- Furnished in the stabilized-annealed condition; Annealing at 927 to 1010°C (1700 to 1850°F); Quenched in water or rapidly cooled by other means
ASTM B 462 N08020 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM B 462 N08020 International Equivalent Materials
Showing 15 of 47 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 47 international equivalents?
See all 47 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 47Cross References
- 11Composition
- 4Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- 20Creep
- -Joints
- -Coatings
- 61Dimensions
- -Tribology
- 8257Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 16Total Suppliers