ASTM B 535 N08332 Nickel Alloys
Data updates
This material has 50 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
ASTM B 535 N08332 Chemical Composition
B535: 2006 / Standard Specification for Nickel-Iron-Chromium-Silicon Alloys (UNS N08330 and N08332) Seamless Pipe and Tube
Looking for full material performance data?
Free registration required • Instant access
ASTM B 535 N08332 Physical Properties
Temperature
This material has 50 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
ASTM B 535 N08332 Heat Treatments
- Annealed; final heat treatment shall be 1150°C (2100°F) minimum.
ASTM B 535 N08332 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
ASTM B 535 N08332 International Equivalent Materials
Showing 10 of 24 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 24 international equivalents?
See all 24 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 24Cross References
- 11Composition
- 5Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- 6Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers