CuNi10Zn42Pb2 (European Union / EN) Material Properties

Other designations:
Material group: Nonferrous Alloys / Copper
Country/Standard: European Union / EN

Data updates

Latest Update: 2022-02
Total number of updates: 5
Update History:
2020-09 2019-06 2014-10 2014-02

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 460 MPa view details
Elongation, A 5 % view details
Shear Strength val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Brinell Hardness (HB) 110 — 190 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 66.7 ksi view details
Elongation, A 5 % view details
Shear Strength val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Brinell Hardness (HB) 110 — 190 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
100 - 300°C
PROPERTY / VALUE
Modulus of Elasticity 100 — 150 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°C
view details
Thermal Conductivity 33.472 W/(m∙°C) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.246 Ω∙mm²/m view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/m
view details
Melting Temperature val1
Full data access requires a free trial. Sign Up Free
°C
view details
Torsional Modulus val1
Full data access requires a free trial. Sign Up Free
GPa
view details
Modulus of Elasticity 14.5 E+03 — 21.8 E+03 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Coefficient of Thermal Expansion (CTE) val1
Full data access requires a free trial. Sign Up Free
10-6/°F
view details
Thermal Conductivity 19.3 BTU/(h∙ft∙°F) view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 409 E-06 Ω∙circular·mil/ft view details
Electrical Conductivity val1
Full data access requires a free trial. Sign Up Free
S/in
view details
Melting Temperature val1
Full data access requires a free trial. Sign Up Free
°F
view details
Torsional Modulus val1
Full data access requires a free trial. Sign Up Free
ksi
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Cu
VALUE
45.0 – 48.0
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
≤ 0.3
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Mn
VALUE
≤ 0.5
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Other total
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Pb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
Sn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-31-5
CRITERIA
Zn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-66-6