C 2700 T (Japan / JIS) Material Properties

Material group: Nonferrous Alloys / Copper
Country/Standard: Japan / JIS

Data updates

Latest Update: 2019-06
Total number of updates: 2
Update History:
2018-04

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Tensile Strength 295 MPa view details
Elongation, A 20 % view details
Rockwell Hardness (HR) 40 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
mm
view details
Tensile Strength 42.8 ksi view details
Elongation, A 20 % view details
Rockwell Hardness (HR) 40 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Grain Size val1
Full data access requires a free trial. Sign Up Free
in
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 100 — 150 GPa view details
Density 7.5 — 9.3 kg/dm³ view details
Modulus of Elasticity 14.5 E+03 — 21.8 E+03 ksi view details
Density 0.271 — 0.336 lb/in³ view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Cu
VALUE
63.0 – 67.0
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
≤ 0.05
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Pb
VALUE
≤ 0.05
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
Zn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-66-6

H 3300: 2018 / Copper and copper alloy seamless pipes and tubes

Heat Treatments