Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
MPa
view details
Tensile Strength 440 MPa view details
Elongation, A 12 % view details
Brinell Hardness (HB) 110 — 160 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 val1
Full data access requires a free trial. Sign Up Free
ksi
view details
Tensile Strength 63.8 ksi view details
Elongation, A 12 % view details
Brinell Hardness (HB) 110 — 160 view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
30 - 100°C
100 - 300°C
PROPERTY / VALUE
Modulus of Elasticity 100 — 150 GPa view details
Density val1
Full data access requires a free trial. Sign Up Free
kg/dm³
view details
Thermal Conductivity 71 W/(m∙°C) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
W/(m∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
J/(kg∙°C)
view details
Electrical Resistivity 0.112 Ω∙mm²/m view details
Electrical Resistivity val1
Full data access requires a free trial. Sign Up Free
Ω∙mm²/m
view details
Melting Temperature val1
Full data access requires a free trial. Sign Up Free
°C
view details
Modulus of Elasticity 14.5 E+03 — 21.8 E+03 ksi view details
Density val1
Full data access requires a free trial. Sign Up Free
lb/in³
view details
Thermal Conductivity 41 BTU/(h∙ft∙°F) view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Thermal Conductivity val1
Full data access requires a free trial. Sign Up Free
BTU/(h∙ft∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Heat Capacity val1
Full data access requires a free trial. Sign Up Free
BTU/(lb∙°F)
view details
Electrical Resistivity 187 E-06 Ω∙circular·mil/ft view details
Electrical Resistivity val1
Full data access requires a free trial. Sign Up Free
Ω∙circular·mil/ft
view details
Melting Temperature val1
Full data access requires a free trial. Sign Up Free
°F
view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Cu
VALUE
66.0 – 70.0
UNIT
%
CAS NUMBER
7440-50-8
CRITERIA
Fe
VALUE
≤ 0.4
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
Ni
VALUE
≤ 0.5
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Other total
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Pb
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-92-1
CRITERIA
Si
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-21-3
CRITERIA
Zn
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-66-6

EN 12449: 2023 / Copper and copper alloys - Seamless, round tubes for general purposes

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now