Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 550 MPa view details
Elongation, A 4 % view details
Yield Strength, Rp0.2 79.8 ksi view details
Elongation, A 4 % view details

Physical Properties


Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Co
VALUE
Remainder
UNIT
%
CAS NUMBER
7440-48-4
CRITERIA
Co+Ni+Cr
VALUE
Co+Ni+Cr >= 85%
UNIT
%
CAS NUMBER
CRITERIA
Cr
VALUE
≥ 25.0000
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mo
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7439-98-7

Dentistry; dental base metal casting alloys (ISO 6871:1987), EN 26871

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now