SAE QE22A Magnesium Alloys
Data updates
This material has 228 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
SAE QE22A Chemical Composition
SAE J465: 2018 / Magnesium casting alloys
Looking for full material performance data?
Free registration required • Instant access
SAE QE22A Physical Properties
Temperature
This material has 228 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
SAE QE22A Heat Treatments
- Solution heat treatment
Heated at 975-995°F (524-535°C). Incremental steps or a uniform heating rate shall be used to prevent eutectic melting which can irreversibly damage castings. A protective atmosphere containing sufficient sulfur dioxide, carbon dioxide, or satisfactory oxidation inhibitor shall be used when solution heat treating at or above 750°F (399°C). Recommended soaking time is 4-8 hours (soaking time starts when all temperature control sensing elements are within 10°F (6°C) of the set or offset temperature). Heavy section castings, t ≥ 25.4 mm, may require longer soaking time than indicated.
Quenched in water (or other suitable media) held at 140-196°F (60-91°C). During the quench, the quenchant temperature shall not rise more than 25°F (14°C).
Aging (precipitation heat treatment)
Temper T6 - artificial aging from the solution heat treated (T4) temper. Heated for 8 hours at 400°F (204°C). Protective atmosphere is not required.
Rework solution heat treatment
Heated at 950°F (510°C). Recommended soaking time is 1-2 hours.
Quenched in water (or other suitable media) held at 140-196°F (60-91°C). - At least one set of tensile specimens shall, during each stage of heat treatment, be placed into a batch-type furnace with each load of castings or into a continuous furnace at intervals of not longer than 3 hours; Tensile Specimens at 400 °F (204 °C): heated to 400 °F ± 5 °F (204 °C ± 3 °C), held at heat for 10 minutes ± 1 minute before testing, and tested at 400 °F ± 5 °F (204 °C ± 3 °C).
SAE QE22A Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
SAE QE22A International Equivalent Materials
Showing 15 of 45 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 45 international equivalents?
See all 45 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 45Cross References
- 13Composition
- 62Mechanical Properties
- 68Physical Properties
- 2Heat Treatment
- -Metallography
- -Machinability
- 24Stress-Strain
- -Formability
- 3Fatigue
- -Fracture
- 1Creep
- 1Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- 4Ageing
- -Weatherability
- -Irradiation
- 5Total Suppliers