TC 340 (Japan / JIS) Material Properties

Material group: Nonferrous Alloys / Titanium
Country/Standard: Japan / JIS

Data updates

Latest Update: 2018-04
Total number of updates: 1
Update History:

Mechanical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Yield Strength, Rp0.2 215 MPa view details
Tensile Strength 340 MPa view details
Elongation, A 15 % view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details
Yield Strength, Rp0.2 31.2 ksi view details
Tensile Strength 49.3 ksi view details
Elongation, A 15 % view details
Vickers Hardness (HV) val1
Full data access requires a free trial. Sign Up Free
view details

Physical Properties


Temperature

0 - 30°C
PROPERTY / VALUE
Modulus of Elasticity 80 — 130 GPa view details
Density 4.3 — 5.1 kg/dm³ view details
Modulus of Elasticity 11.6 E+03 — 18.9 E+03 ksi view details
Density 0.155 — 0.184 lb/in³ view details

Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
≤ 0.10
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Fe
VALUE
≤ 0.25
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
H
VALUE
≤ 0.015
UNIT
%
CAS NUMBER
1333-74-0
CRITERIA
N
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
O
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7782-44-7; 17778-80-2
CRITERIA
Other each
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Other total
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
CRITERIA
Ti
VALUE
val1
Full data access requires a free trial. Sign Up Free
UNIT
%
CAS NUMBER
7440-32-6

H 5801: 2000 / Titanium and titanium alloy castings

Heat Treatments

Since direct data is not available in the original source, register for a free trial to explore similar or equivalent materials having these properties.

Register Now