SAE Ti-6Al-2Sn-4Zr-6Mo Titanium Alloys

Material group: Nonferrous Alloys / Titanium Alloys
Country / Standard: United States / SAE

Data updates

Latest Update: 2023-05
Total number of updates: 8
Update History

This material has 4529 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

SAE Ti-6Al-2Sn-4Zr-6Mo Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
Al
VALUE
5.50 – 6.50
UNIT
%
CAS NUMBER
7429-90-5
CRITERIA
C
VALUE
≤ 0.04
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Fe
VALUE
≤ 0.15
UNIT
%
CAS NUMBER
7439-89-6
CRITERIA
H
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
1333-74-0
CRITERIA
Mo
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7439-98-7
CRITERIA
N
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7727-37-9; 17778-88-0
CRITERIA
O
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7782-44-7; 17778-80-2
CRITERIA
Other each
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
CRITERIA
Other total
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
CRITERIA
Sn
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-31-5
CRITERIA
Ti
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-32-6
CRITERIA
Y
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-65-5
CRITERIA
Zr
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-67-7

SAE AMS 4981J: 2022 / Titanium Alloy Bars, Wire, and Forgings 6.0Al - 2.0Sn - 4.0Zr - 6.0Mo Solution and Precipitation Heat Treated

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

SAE Ti-6Al-2Sn-4Zr-6Mo Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
80 — 130 GPa
Unlock full details
Full data available with free access View Complete Material Data
Electrical Resistivity
2 Ω∙mm²/m
Unlock full details
Full data available with free access View Complete Material Data
Density
val1
Full data available with free access View Complete Material Data
kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Electrical Conductivity
val1
Full data available with free access View Complete Material Data
S/m
Unlock full details
Full data available with free access View Complete Material Data
Heat Capacity
val1
Full data available with free access View Complete Material Data
J/(kg∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Thermal Conductivity
7.7 W/(m∙°C)
Unlock full details
Full data available with free access View Complete Material Data

This material has 4529 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

SAE Ti-6Al-2Sn-4Zr-6Mo Heat Treatments


  • Bars and forgings 12.7 mm and over in nominal diameter or least distance between parallel sides shall be solution heat treated by heating in a suitable atmosphere to 816 to 913°C (1500 to 1675 °F), holding at the selected temperature within ±14°C (±25 °F) for not less than 1 hour, and cooling at a rate equivalent to an air cool or faster, and precipitation heat treated by heating to 593°C ± 8 (1100 °F ± 15 °F), holding at heat for 4 to 8 hours, and cooling in air. Heat treatment for product under 12.7 mm nominal diameter or least distance between parallel sides shall be as agreed upon by purchaser and vendor.
  • Bars and forgings shall be solution heat treated at 816 to 913°C (1500 to 1675°F) holding at the selected temperature within ±14°C (±25°F) for a time commensurate with section thickness and the heating equipment and procedure used, and water quenched (except that thin sections may be air cooled) and aged at 566 to 677°C (1050 to 1250°F) hold at the selected temperature within ±8°C (±15°F) for 4 to 8 hours.

SAE Ti-6Al-2Sn-4Zr-6Mo Mechanical Properties


Temperature

PROPERTY / VALUE
Tensile Strength
≥ 1034 MPa
Unlock full details
Full data available with free access View Complete Material Data
Elongation, A
≥ 6 %
Unlock full details
Full data available with free access View Complete Material Data
Yield Strength, Rp0.2
val1
Full data available with free access View Complete Material Data
MPa
Unlock full details
Full data available with free access View Complete Material Data
Reduction of Area
val1
Full data available with free access View Complete Material Data
%
Unlock full details
Full data available with free access View Complete Material Data

Need complete mechanical properties to make the right choice?

Get complete data on strength, hardness, fatigue, and more.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

SAE Ti-6Al-2Sn-4Zr-6Mo International Equivalent Materials


Showing 5 of 12 results.

MATERIAL
STANDARD
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
MATERIAL
STANDARD
UNS
COUNTRY / PRODUCER
United States
EQUIVALENCE CATEGORY
Official
STANDARD
GB
COUNTRY / PRODUCER
China
EQUIVALENCE CATEGORY
Official
STANDARD
MIL
COUNTRY / PRODUCER
United States
EQUIVALENCE CATEGORY
Official
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit

Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.

Need the full list of 12 international equivalents?

See all 12 equivalent grades with detailed mapping by standard, producer and equivalence category.

View All Equivalents ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 12Cross References

  • 51Composition
  • 69Mechanical Properties
  • 13Physical Properties
  • 5Heat Treatment
  • -Metallography
  • -Machinability

  • 26Stress-Strain
  • -Formability
  • 24Fatigue
  • 2Fracture
  • 1Creep

  • -Joints
  • -Coatings
  • 29Dimensions
  • -Tribology

  • 4283Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 14Total Suppliers