AA 2117 Aluminium Alloys
Data updates
This material has 279 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
AA 2117 Chemical Composition
International alloy designations and chemical composition limits for wrought aluminum and wrought aluminum alloys - Teal Sheets (2025), 2025
Looking for full material performance data?
Free registration required • Instant access
AA 2117 Physical Properties
Temperature
This material has 279 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
AA 2117 Heat Treatments
- The times and temperatures are typical for various forms, sizes and methods of manufacture and may not exactly describe the optimum treatment for a specific item.
The nominal temperatures at which metal is heated (applies both for solution and precipitation heat treatment) should be attained as rapidly as possible and maintained ± 5°C of nominal during the time at temperature.
Material should be quenched from the solution heat-treating temperature as rapidly as possible and with minimum delay after removal from the furnace. Quenching is typically performed by immersion of wrought products in a cold water bath, although some forgings are quenched in hot-water. Quenching may be performed by alternative means such as total immersion in an aqueous polymer solution, liquefied gas, hot water, or boiling water, or by air blast or fog to minimize distortion provided samples from the material. The use of high-velocity high-volume jets of cold water is also effective for some materials.
For rolled or cold finished wire and rod
Temper T4: Solution heat treated at 500°C, quenched, naturally aged.
Temper T42: Solution heat treated at 500°C, quenched, naturally aged.
Annealing (O)
Heated at 415°C, held for 2-3 hours. This treatment is intended to remove effects of solution heat treatment and include cooling at a rate of about 30°C per hour from the annealing temperature to 260°C. The rate of subsequent cooling is unimportant. Treatment at 345°C, followed by uncontrolled cooling, may be used to remove the effects of cold work, or to partially remove the effects of heat treatment.
AA 2117 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
AA 2117 International Equivalent Materials
Showing 15 of 91 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 91 international equivalents?
See all 91 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 91Cross References
- 20Composition
- 48Mechanical Properties
- 26Physical Properties
- 1Heat Treatment
- -Metallography
- 1Machinability
- 3Stress-Strain
- 1Formability
- 4Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- 40Ageing
- -Weatherability
- -Irradiation
- 44Total Suppliers