PROPRIETARY SAF 2205 SH Chemical Composition
Alleima, Product Data Sheets,
Looking for full material performance data?
Free registration required • Instant access
PROPRIETARY SAF 2205 SH Physical Properties
Temperature
This material has 62 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
PROPRIETARY SAF 2205 SH Heat Treatments
- For batch tempering: 450°C (840°F) for 1 - 3 h. When tempering in a continuous conveyor furnace, where holding time at full temperature is very short, the temperature should be increased to about 500°C (930°F) and the holding time should be 3 - 10 minutes.
PROPRIETARY SAF 2205 SH Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
PROPRIETARY SAF 2205 SH International Equivalent Materials
Showing 3 of 11 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 11 international equivalents?
See all 11 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 11Cross References
- 9Composition
- 14Mechanical Properties
- 23Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 4Total Suppliers