TU VKS170 Structural and constructional steels
Data updates
This material has 20 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
TU VKS170 Chemical Composition
TU 14-1-3404: 1982 / Hot-rolled bars from steel grade 03N18K8M5T-VD (EK21-VD, VKS170-VD)
Looking for full material performance data?
Free registration required • Instant access
TU VKS170 Physical Properties
Temperature
This material has 20 properties — only a subset is shown here.
Unlock detailed physical values across temperatures and conditions.
Free registration required • Instant access
TU VKS170 Heat Treatments
- Hardening at 780-800°С for 1 hour, cooling in air, aging at 500 ± 10°C, 2-8 h, cooling in air.
TU VKS170 Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
TU VKS170 International Equivalent Materials
Showing 1 of 1 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 1 international equivalents?
See all 1 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 1Cross References
- 11Composition
- 4Mechanical Properties
- 3Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers