KS C26-52L Cast steels
Data updates
This material has 64 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
KS C26-52L Chemical Composition
D ISO 4991: 2004 / Steel castings for pressure purposes
Looking for full material performance data?
Free registration required • Instant access
KS C26-52L Heat Treatments
- Normalized and tempered (N+T): Austenitized at 890-980°C, air cooled. Tempered at 600-700°C, air or furnace cooled
Quenched and tempered (Q+T): Austenitized at 890-980°C, liquid quenched. Tempered at 600-700°C, air or furnace cooled
KS C26-52L Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
KS C26-52L International Equivalent Materials
Showing 1 of 54 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 54 international equivalents?
See all 54 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 54Cross References
- 5Composition
- 4Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- -Total Suppliers