KS C23-45A Cast steels
Data updates
This material has 69 properties — only a subset is shown here.
Unlock full material properties, including detailed values across temperatures and conditions.
Free registration required • Instant access
KS C23-45A Chemical Composition
D ISO 4991: 2004 / Steel castings for pressure purposes
Looking for full material performance data?
Free registration required • Instant access
KS C23-45A Heat Treatments
- Annealed (A): Austenitized at 890-980°C, furnace cooled
Normalized and tempered (N+T): Austenitized at 890-980°C, air cooled. Tempered at 600-700°C
Quenched and tempered (Q+T): Austenitized at 890-980°C, liquid quenched. Tempered at 600-700°C
KS C23-45A Mechanical Properties
Temperature
Need complete mechanical properties to make the right choice?
Get complete data on strength, hardness, fatigue, and more.
Free registration required • Instant access
KS C23-45A International Equivalent Materials
Showing 8 of 56 results.
Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.
Need the full list of 56 international equivalents?
See all 56 equivalent grades with detailed mapping by standard, producer and equivalence category.
Free registration required • Instant access
Optimize material selection for your application - Book A Demo
- 56Cross References
- 5Composition
- 5Mechanical Properties
- -Physical Properties
- 1Heat Treatment
- -Metallography
- -Machinability
- -Stress-Strain
- -Formability
- -Fatigue
- -Fracture
- -Creep
- -Joints
- -Coatings
- -Dimensions
- -Tribology
- -Corrosion
- -Ageing
- -Weatherability
- -Irradiation
- 2Total Suppliers