PROPRIETARY HC16S Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2022-05
Total number of updates: 1
Update History

This material has 30 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY HC16S Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
0.33
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
16.00
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
S
VALUE
0.08
UNIT
%
CAS NUMBER
7704-34-9

Dörrenberg Edelstahl GmbH, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY HC16S Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Thermal Conductivity
17 W/(m∙°C)
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
val1
Full data available with free access View Complete Material Data
Unlock full details
Full data available with free access View Complete Material Data

This material has 30 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY HC16S Heat Treatments


  • Soft annealed: 750-850°C, furnace cooled (HB ≤ 280)
    Stress relief annealed: 500-550°C, furnace cooled
    Hardened: 1000-1030°C, oil cooled, pressure gas (N2) or air

    Stress relief annealing recommendation 500-550°C is valid for quenched and tempered condition. In the soft annealed condition stress relieving between 600-650°C is possible.

PROPRIETARY HC16S International Equivalent Materials


Showing 6 of 7 results.

MATERIAL
STANDARD
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit
MATERIAL
STANDARD
PROPRIETARY
COUNTRY / PRODUCER
EQUIVALENCE CATEGORY
Implicit

Equivalence categories reflect chemical-composition and mechanical-property comparison — always verify suitability against the governing specification for your application.

Need the full list of 7 international equivalents?

See all 7 equivalent grades with detailed mapping by standard, producer and equivalence category.

View All Equivalents ›
Free registration required • Instant access

Free registration required • Instant access

Book A Demo

Optimize material selection for your application - Book A Demo

  • 7Cross References

  • 3Composition
  • -Mechanical Properties
  • 8Physical Properties
  • 4Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 8Total Suppliers