PROPRIETARY SIHARD 3501 Tool steels

Material group: Ferrous Alloys / Tool steels
Country / Standard: PROPRIETARY

Data updates

Latest Update: 2021-11
Total number of updates: 1
Update History

This material has 12 properties — only a subset is shown here.

Unlock full material properties, including detailed values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY SIHARD 3501 Chemical Composition

CRITERIA
VALUE
UNIT
CAS NUMBER
CRITERIA
C
VALUE
1.00
UNIT
%
CAS NUMBER
7440-44-0
CRITERIA
Cr
VALUE
0.50
UNIT
%
CAS NUMBER
7440-47-3
CRITERIA
Mn
VALUE
0.35
UNIT
%
CAS NUMBER
7439-96-5
CRITERIA
Ni
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-02-0
CRITERIA
Si
VALUE
val1
Full data available with free access View Complete Material Data
UNIT
%
CAS NUMBER
7440-21-3

SIJ Metal Ravne, Product Data Sheets,

Looking for full material performance data?

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY SIHARD 3501 Physical Properties


Temperature

PROPERTY / VALUE
Modulus of Elasticity
190 — 210 GPa
Unlock full details
Full data available with free access View Complete Material Data
Density
7.72 — 8 kg/dm³
Unlock full details
Full data available with free access View Complete Material Data
Poisson Coefficient
0.27 — 0.3
Unlock full details
Full data available with free access View Complete Material Data

This material has 12 properties — only a subset is shown here.

Unlock detailed physical values across temperatures and conditions.

View Complete Material Data ›
Free registration required • Instant access

Free registration required • Instant access

PROPRIETARY SIHARD 3501 Heat Treatments


  • Soft annealing: Heat to 730-760°C, cool slowly. This will produce a maximum Brinell hardness of 207.
    Stress relieving: Stress relieving to remove machining stresses should be carried out by heating to approx. 600-650°C, holding for 1-2 hours at heat, followed by air cooling. This operation is performed to reduce distortion during heat treatment.
    Hardening: Harden from a temperature of 780-810°C, 820-850°C followed by water or oil quenching. Hardness after quenching is about 60 HRC.
    Tempering temperature: 150-180°C.

Optimize material selection for your application - Book A Demo

  • -Cross References

  • 5Composition
  • -Mechanical Properties
  • 5Physical Properties
  • 1Heat Treatment
  • -Metallography
  • -Machinability

  • -Stress-Strain
  • -Formability
  • -Fatigue
  • -Fracture
  • -Creep

  • -Joints
  • -Coatings
  • -Dimensions
  • -Tribology

  • -Corrosion
  • -Ageing
  • -Weatherability
  • -Irradiation

  • 1Total Suppliers